AEM
Home Help [Feedback] [For Subscribers] [Archive] [Search] [Contents]
This Article
Right arrow Full Text
Right arrow Full Text (PDF)
Right arrow Alert me when this article is cited
Right arrow Alert me if a correction is posted
Services
Right arrow Similar articles in this journal
Right arrow Similar articles in PubMed
Right arrow Alert me to new issues of the journal
Right arrow Download to citation manager
Right arrowReprints and Permissions
Right arrow Copyright Information
Right arrow Books from ASM Press
Right arrow MicrobeWorld
Citing Articles
Right arrow Citing Articles via HighWire
Right arrow Citing Articles via Google Scholar
Google Scholar
Right arrow Articles by Nagaoka, T.
Right arrow Articles by Saiki, H.
Right arrow Search for Related Content
PubMed
Right arrow PubMed Citation
Right arrow Articles by Nagaoka, T.
Right arrow Articles by Saiki, H.
Agricola
Right arrow Articles by Nagaoka, T.
Right arrow Articles by Saiki, H.

 Previous Article  |  Next Article 

Applied and Environmental Microbiology, August 1999, p. 3588-3593, Vol. 65, No. 8
0099-2240/99/$04.00+0
Copyright © 1999, American Society for Microbiology. All rights reserved.

A Novel Mineral Flotation Process Using Thiobacillus ferrooxidans

Toru Nagaoka, Naoya Ohmura,* and Hiroshi Saiki

Department of Bio-Science, Central Research Institute of Electric Power Industry, 1646 Abiko, Abiko City, Chiba, Japan

Received 2 March 1999/Accepted 20 May 1999

Oxidative leaching of metals by Thiobacillus ferrooxidans has proven useful in mineral processing. Here, we report on a new use for T. ferrooxidans, in which bacterial adhesion is used to remove pyrite from mixtures of sulfide minerals during flotation. Under control conditions, the floatabilities of five sulfide minerals tested (pyrite, chalcocite, molybdenite, millerite, and galena) ranged from 90 to 99%. Upon addition of T. ferrooxidans, the floatability of pyrite was significantly suppressed to less than 20%. In contrast, addition of the bacterium had little effect on the floatabilities of the other minerals, even when they were present in relatively large quantities: their floatabilities remained in the range of 81 to 98%. T. ferrooxidans thus appears to selectively suppress pyrite floatability. As a consequence, 77 to 95% of pyrite was removed from mineral mixtures while 72 to 100% of nonpyrite sulfide minerals was recovered. The suppression of pyrite floatability was caused by bacterial adhesion to pyrite surfaces. When normalized to the mineral surface area, the number of cells adhering to pyrite was significantly larger than the number adhering to other minerals. These results suggest that flotation with T. ferrooxidans may provide a novel approach to mineral processing in which the biological functions involved in cell adhesion play a key role in the separation of minerals.


* Corresponding author. Mailing address: Central Research Institute of Electric Power Industry, 1646 Abiko, Abiko City, Chiba, Japan. Phone: 81-471-82-1181. Fax: 81-471-83-3347. E-mail: ohmura{at}criepi.denken.or.jp.


Applied and Environmental Microbiology, August 1999, p. 3588-3593, Vol. 65, No. 8
0099-2240/99/$04.00+0
Copyright © 1999, American Society for Microbiology. All rights reserved.



This article has been cited by other articles:




Home Help [Feedback] [For Subscribers] [Archive] [Search] [Contents]
J. Bacteriol. Microbiol. Mol. Biol. Rev. Eukaryot. Cell All ASM Journals

Copyright © 1999 by the American Society for Microbiology. All rights reserved.